    • Remove the borosilicate glass from your printer.

    • Test fit the PEI on the bed glass so you see how it will fit.

    • Thoroughly clean both sides of the glass with isopropyl alcohol and dry with a lint-free cloth.

    • Peal away about 2cm (1") of backing from one edge of the PEI and attach it to the glass. position the PEI as precisely as you can - once the adhesive touches the glass, it can't be moved.

    • Smooth the adhered section with the edge of a soft plastic scraper or credit card. Then, slowly remove the backing as you advance and smooth the PEI with the scraper until it is completely adhered. Smooth the entire sheet from the center to the edges radially, to firmly adhere it.

    • The PT100 probes are much more accurate than a thermistor and can handle temperatures up to 400°C for printing high temp materials like Delrin and Polycarbonate.